Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | 5.60e+14 ohm | 5.60e+14 ohm | ASTM D257 |
Lubrizol Estane® ZHF 95AT3 Thermoplastic Polyurethane, Flame Retardant Type: Estane® ZHF 95AT3 TPU is a zero halogen flame retardant polyether based thermoplastic polyurethane compound.Features: Outstanding flame retardant properties, especially suited for tray cables.. |