Polymer Property : Surface Resistivity per Square = 4100 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistivity per Square 4100 ohm
4100 ohm
Applied Coating; 6 micron wet film
Heraeus Cleviosâ„¢ P T2 Conductive Sulfonate Polymer for Antistatic Coatings
Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as an aqueous dispersion used to produce thin film antistatic coatings. Cleviosâ„¢ P T2 is an antistatic material based on PEDOT:..