Electrical Properties Metric English Comments
Surface Resistivity per Square 4000 ohm
4000 ohm
2.5 wt% carbon nanotubes in PC; CTM E042
Nanocyl PLASTICYL™ PC1501 Polycarbonate with 2 wt% Multi-Wall Carbon Nanotubes
PLASTICYL™ is a family of Multi-Wall Carbon Nanotube (MWNT) thermoplastic concentrates for applications requiring superior electrical conductivity and electrostatic discharge (ESD) properties. PLA..
Surface Resistivity per Square 4000 ohm
4000 ohm
2.5 wt% carbon nanotubes in PC; CTM E042
Nanocyl PLASTICYL™ PC1501 Polycarbonate with 3 wt% Multi-Wall Carbon Nanotubes
PLASTICYL™ is a family of Multi-Wall Carbon Nanotube (MWNT) thermoplastic concentrates for applications requiring superior electrical conductivity and electrostatic discharge (ESD) properties. PLA..