Polymer Property : Surface Resistivity per Square = 4.80e+8 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistivity per Square 4.80e+8 ohm
4.80e+8 ohm
50%; ASTM D257
Lubrizol STAT-RITE® S-1107 Static Dissipative TPU
Description: Stat-Rite® S-1107 is a static dissipative TPU alloy. Stat-Rite S-1107 utilizes the patented Stat-Rite inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD ..