Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | 3.80e+17 ohm | 3.80e+17 ohm | ASTM D-257 |
Saint-Gobain Norton® Fluorglas® Chemfilm® DF2929 Fluoropolymer Tape Description: Chemfilm® Fluoropolymer Cast Films and Tapes for Wire and Cable Industry: Multi-layer cast film process ensures inherently pin-hole free structure, therefore cast films possess super.. |