Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | 3.70e+10 ohm | 3.70e+10 ohm | |
Mykroy/Mycalex MM 451 Molding Grade Glass-bonded Mica Composite Natural mica filler. Does not burn. ROHS Compliant.This ceramoplastic material is a versatile and efficient insulating material designed to meet the exacting demands of technical markets, worldwid.. |