Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | 110000 ohm | 110000 ohm | ASTM D257 |
PolyOne Therma-Tech™ NJC-8500 Nylon 12
(discontinued **) PolyOne First ChoiceInformation provided by PolyOne Corporation. |