Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | 1.50e+10 ohm | 1.50e+10 ohm | ASTM D257 |
Lubrizol ESTANE® T5192 Ether-Type Dissipative Compound (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |