Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | 1.00e+6 - 1.00e+8 ohm | 1.00e+6 - 1.00e+8 ohm | ASTM D257; DIN 53482 |
Kleerdex Elson® 405 AS DC Plate, PMMA/Acrylic, Clear Transparent