Electrical Properties Metric English Comments
Surface Resistivity per Square 1.00e+7 - 1.00e+10 ohm
1.00e+7 - 1.00e+10 ohm
ASTM D257
Quadrant EPP TIVAR® CleanStat™ FDA, USDA, 3-A Dairy, Electro Static Dissipative UHMW-PE (ASTM Product Data Sheet)
Surface Resistivity per Square 1.00e+9 - 1.00e+10 ohm
1.00e+9 - 1.00e+10 ohm
EOS/ESD S11.11
Quadrant EPP Semitron® ESd 225, Extruded, Static Dissipative Acetal (ASTM Product Data Sheet)