Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | 0.60 ohm | 0.60 ohm | |
Parker Chomerics PREMIER™ A230-FRHF EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |
|||
Surface Resistivity per Square | 0.60 ohm | 0.60 ohm | |
Parker Chomerics PREMIER™ A230-HTHF EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |
|||
Surface Resistivity per Square | 0.60 ohm | 0.60 ohm | cured film; 23 microns thick |
Gwent Electronic Materials C2000215D4 Silver / Silver Chloride Paste C2000215D4 has a ratio of Silver to Silver Chloride of 50/50. This is used for reference electrodes in Medical Diagnostics, Environmental Sensor and the "Agri-Food" Industries. It forms part of a .. |
|||
Surface Resistivity per Square | <= 0.60 ohm | <= 0.60 ohm | |
Abatron AboWeld 8709-18/AboCure 50-12 Nickel-Filled Electrically Conductive Epoxy Compound AboWeld 8709-18/AboCure 50-12 is a practically solventless nickel-epoxy adhesive and resurfacing system with good coating capabilities in the intermediate conductivity range. It is very versatile. |