Polymer Property : Surface Resistivity per Square = 0.075 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistivity per Square <= 0.075 ohm
<= 0.075 ohm
CEPS-0002
Parker Chomerics CHO-SHIELD® 4994 Conductive Flexible Coating
Description: CHO-SHIELD® 4994 is a smooth, highly conductive flexible silver-filled polyurethane coating designed for military/aerospace airframe applications. Both coatings provide superior adhesi..
Surface Resistivity per Square <= 0.075 ohm

@Temperature 22.2 °C,
Time 1.21e+6 sec
<= 0.075 ohm

@Temperature 72.0 °F,
Time 336 hour
MIL-T-5624 JP-8; CEPS-0002
Parker Chomerics CHO-SHIELD® 4994 Conductive Flexible Coating
Description: CHO-SHIELD® 4994 is a smooth, highly conductive flexible silver-filled polyurethane coating designed for military/aerospace airframe applications. Both coatings provide superior adhesi..
Surface Resistivity per Square <= 0.075 ohm

@Temperature 71.1 °C,
Time 605000 sec
<= 0.075 ohm

@Temperature 160 °F,
Time 168 hour
MIL-H-5606 Hydraulic Fluid; CEPS-0002
Parker Chomerics CHO-SHIELD® 4994 Conductive Flexible Coating
Description: CHO-SHIELD® 4994 is a smooth, highly conductive flexible silver-filled polyurethane coating designed for military/aerospace airframe applications. Both coatings provide superior adhesi..
Surface Resistivity per Square <= 0.075 ohm

@Temperature 71.1 °C,
Time 605000 sec
<= 0.075 ohm

@Temperature 160 °F,
Time 168 hour
MIL-L-7808 Lubrication Oil; CEPS-0002
Parker Chomerics CHO-SHIELD® 4994 Conductive Flexible Coating
Description: CHO-SHIELD® 4994 is a smooth, highly conductive flexible silver-filled polyurethane coating designed for military/aerospace airframe applications. Both coatings provide superior adhesi..
Surface Resistivity per Square <= 0.075 ohm

@Temperature 85.0 °C,
Time 1.21e+6 sec
<= 0.075 ohm

@Temperature 185 °F,
Time 336 hour
CEPS-0002
Parker Chomerics CHO-SHIELD® 4994 Conductive Flexible Coating
Description: CHO-SHIELD® 4994 is a smooth, highly conductive flexible silver-filled polyurethane coating designed for military/aerospace airframe applications. Both coatings provide superior adhesi..
Surface Resistivity per Square <= 0.075 ohm

@Temperature -40.0 °C,
Time 1.21e+6 sec
<= 0.075 ohm

@Temperature -40.0 °F,
Time 336 hour
CEPS-0002
Parker Chomerics CHO-SHIELD® 4994 Conductive Flexible Coating
Description: CHO-SHIELD® 4994 is a smooth, highly conductive flexible silver-filled polyurethane coating designed for military/aerospace airframe applications. Both coatings provide superior adhesi..
Surface Resistivity per Square <= 0.075 ohm

@Temperature 85.0 °C,
Time 2.59e+6 sec
<= 0.075 ohm

@Temperature 185 °F,
Time 720 hour
CEPS-0002
Parker Chomerics CHO-SHIELD® 4994 Conductive Flexible Coating
Description: CHO-SHIELD® 4994 is a smooth, highly conductive flexible silver-filled polyurethane coating designed for military/aerospace airframe applications. Both coatings provide superior adhesi..
Surface Resistivity per Square <= 0.075 ohm
<= 0.075 ohm
CEPS-0002
Parker Chomerics CHO-SHIELD® 4998 Conductive Flexible Coating
Description: CHO-SHIELD® 4998 is a smooth, highly conductive flexible silver-filled polyurethane coating designed for military/aerospace airframe applications. Both coatings provide superior adhesi..
Surface Resistivity per Square <= 0.075 ohm

@Temperature 22.2 °C,
Time 1.21e+6 sec
<= 0.075 ohm

@Temperature 72.0 °F,
Time 336 hour
MIL-T-5624 JP-8; CEPS-0002
Parker Chomerics CHO-SHIELD® 4998 Conductive Flexible Coating
Description: CHO-SHIELD® 4998 is a smooth, highly conductive flexible silver-filled polyurethane coating designed for military/aerospace airframe applications. Both coatings provide superior adhesi..
Surface Resistivity per Square <= 0.075 ohm

@Temperature 71.1 °C,
Time 605000 sec
<= 0.075 ohm

@Temperature 160 °F,
Time 168 hour
MIL-H-5606 Hydraulic Fluid; CEPS-0002
Parker Chomerics CHO-SHIELD® 4998 Conductive Flexible Coating
Description: CHO-SHIELD® 4998 is a smooth, highly conductive flexible silver-filled polyurethane coating designed for military/aerospace airframe applications. Both coatings provide superior adhesi..
Surface Resistivity per Square <= 0.075 ohm

@Temperature 71.1 °C,
Time 605000 sec
<= 0.075 ohm

@Temperature 160 °F,
Time 168 hour
MIL-L-7808 Lubrication Oil; CEPS-0002
Parker Chomerics CHO-SHIELD® 4998 Conductive Flexible Coating
Description: CHO-SHIELD® 4998 is a smooth, highly conductive flexible silver-filled polyurethane coating designed for military/aerospace airframe applications. Both coatings provide superior adhesi..
Surface Resistivity per Square <= 0.075 ohm

@Temperature 85.0 °C,
Time 1.21e+6 sec
<= 0.075 ohm

@Temperature 185 °F,
Time 336 hour
CEPS-0002
Parker Chomerics CHO-SHIELD® 4998 Conductive Flexible Coating
Description: CHO-SHIELD® 4998 is a smooth, highly conductive flexible silver-filled polyurethane coating designed for military/aerospace airframe applications. Both coatings provide superior adhesi..
Surface Resistivity per Square <= 0.075 ohm

@Temperature -40.0 °C,
Time 1.21e+6 sec
<= 0.075 ohm

@Temperature -40.0 °F,
Time 336 hour
CEPS-0002
Parker Chomerics CHO-SHIELD® 4998 Conductive Flexible Coating
Description: CHO-SHIELD® 4998 is a smooth, highly conductive flexible silver-filled polyurethane coating designed for military/aerospace airframe applications. Both coatings provide superior adhesi..
Surface Resistivity per Square <= 0.075 ohm

@Temperature 85.0 °C,
Time 2.59e+6 sec
<= 0.075 ohm

@Temperature 185 °F,
Time 720 hour
CEPS-0002
Parker Chomerics CHO-SHIELD® 4998 Conductive Flexible Coating
Description: CHO-SHIELD® 4998 is a smooth, highly conductive flexible silver-filled polyurethane coating designed for military/aerospace airframe applications. Both coatings provide superior adhesi..