Polymer Property : Surface Resistivity per Square = 0.0060 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistivity per Square 0.0060 ohm

@Thickness 0.0150 mm
0.0060 ohm

@Thickness 0.000591 in
Using a 230 mesh stainless steel screen
Gwent Electronic Materials C2050926P2 Lead-free Ag PZT Paste
This product is a Lead free termination for single layer PZT ceramics. After firing the film has good adhesion and solderability. Screen Printing Equipment: semi-automatic, manualScreen Types: stai..