Electrical Properties Metric English Comments
Comparative Tracking Index 550 - 604 V
550 - 604 V
Average value: 594 V Grade Count:8
Overview of materials for Nylon 6, MoS2 Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria..