Electrical Properties | Metric | English | Comments |
---|---|---|---|
Comparative Tracking Index | 601 V | 601 V | IEC 60112 |
Menzolit Menzolit® SMC 0430 Unsaturated Polyester UP SMC 0430 is a low emission Class-A SMC for on-line painted exterior body applications on passenger cars. These compounds mould to parts with excellent surface quality for on-line painted body panel.. |
|||
Comparative Tracking Index | 601 V | 601 V | IEC 60112 |
Menzolit Menzolit® BMC 2900 Unsaturated Polyester UP BMC 2900 is a specially designed BMC to meet the EC Safety Signs Directive (92/58/EEC) on the provision and use of safety signs at work. In areas where it is not possible to include the use of illu.. |