Electrical Properties | Metric | English | Comments |
---|---|---|---|
Comparative Tracking Index | 370 V @Temperature 23.0 °C |
370 V @Temperature 73.4 °F |
IEC 60112 |
DuPont Performance Polymers Crastin® SK615SF NC010 PBT
(Unverified Data**) Crastin® SK615SF is a 30% glass fiber reinforced, low viscosity polybutylene terephthalate for injection molding. It has high flow characteristics and is specifically suitable for super fast produc.. |