Electrical Properties | Metric | English | Comments |
---|---|---|---|
Comparative Tracking Index | 305 V | 305 V | IEC 112 |
Wolf Kunststoff ZEDEX® ZX-100K A1K Polymer Alloy Main Characteristics: Hard; Stiff; Tough; High fatigue strength; Good weather resistance; Good machinability; FDA compliant LABS; PTFE and silicone-free; KTW approved; Stress resistantApplications: .. |