Polymer Property : Comparative Tracking Index = 170 V Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Comparative Tracking Index 170 V

@Thickness 3.17 mm
170 V

@Thickness 0.125 in
ASTM D3638
Industrial Laminates/Norplex NP320 Cotton Fabric
Description: Fine weave (less than 4 ounce/square yard) cotton fabric commonly called linen, combined with phenolic resin to provide better machining than NP310. For smaller and more intricate shape..
Comparative Tracking Index 170 V

@Thickness 3.17 mm
170 V

@Thickness 0.125 in
ASTM D3638
Industrial Laminates/Norplex NP320E Cotton Fabric
Description: Similar to NP320 with improved moisture resistance. Suitable for electrical applications in moderate humidity conditions.Thickness Tested: 0.062", 0.125", and 0.500”
Comparative Tracking Index 170 V

@Thickness 3.17 mm
170 V

@Thickness 0.125 in
ASTM D3638
Industrial Laminates/Norplex NP320U Cotton Fabric
Description: Utility version of NP320E. Meets most, but not all, NEMA properties for L and LE, and is not certifiable as a NEMA Grade.Thickness Tested: 0.062", 0.125", and 0.500"