Electrical Properties | Metric | English | Comments |
---|---|---|---|
Magnetic Maximum Energy Product, BH | 31 - 33 MGOe | 31 - 33 MGOe | |
Alliance N-33 Neodymium Iron Boron Magnetic Material |
|||
Magnetic Maximum Energy Product, BH | 31 - 33 MGOe | 31 - 33 MGOe | |
Alliance N-33M Neodymium Iron Boron Magnetic Material |