Electrical Properties | Metric | English | Comments |
---|---|---|---|
Magnetic Maximum Energy Product, BH | 3.6 MGOe | 3.6 MGOe | |
Alliance C-8 Strontium Ferrite Ceramic Magnetic Material |
|||
Magnetic Maximum Energy Product, BH | 3.6 MGOe | 3.6 MGOe | |
Alliance BIN-26 Bonded (Composite) Magnetic Material |