Polymer Property : Magnetic Maximum Energy Product, BH = 29 MGOe Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Magnetic Maximum Energy Product, BH 26 - 29 MGOe
26 - 29 MGOe
Alliance N-28EH Neodymium Iron Boron Magnetic Material
Magnetic Maximum Energy Product, BH 26 - 29 MGOe
26 - 29 MGOe
Alliance N-28UH Neodymium Iron Boron Magnetic Material