Electrical Properties | Metric | English | Comments |
---|---|---|---|
Magnetic Maximum Energy Product, BH | 24 - 26 MGOe | 24 - 26 MGOe | |
Ceradyne SEMICORE® S2-17A MMPA 24/18 Sm2 (CoFeCuZr)17 Samarium Cobalt Magnet Magnetic alignment at 90° to Compaction AxisApplications:Microwave amplifiers and oscillators for airborne equipmentTWT modules for phased array radarSmall motors for severe thermal conditions Herm.. |