Electrical Properties | Metric | English | Comments |
---|---|---|---|
Magnetic Maximum Energy Product, BH | 16 - 18 MGOe | 16 - 18 MGOe | |
Ceradyne SEMICORE® S1-5B MMPA 16/18 SmCo5 Samarium Cobalt Magnet Magnetic alignment parallel to Compaction AxisApplications:Microwave amplifiers and oscillators for airborne equipmentTWT modules for phased array radarSmall motors for severe thermal conditions Her.. |