Electrical Properties | Metric | English | Comments |
---|---|---|---|
Magnetic Maximum Energy Product, BH | 0.40 MGOe | 0.40 MGOe | |
LATI Latamid 12 H FE90 PA 12, Heat Stabilized Polyamide 12 (PA12) based compound. Heat stabilized. Magnetizable filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria.. |