Electrical Properties | Metric | English | Comments |
---|---|---|---|
Insulation Resistance | 8.58e+9 ohm @Time 605000 sec |
8.58e+9 ohm @Time 168 hour |
Control; IPC B24 |
Indium Corp. WF-9945 Wave Solder Flux, Halogen-Free WF-9945 is a halogen-free no-clean flux developed for wave soldering mixed-technology and through-hole electronics assemblies.WF-9945 is formulated to provide a excellent wetting and superior hole-f.. |