Electrical Properties | Metric | English | Comments |
---|---|---|---|
Insulation Resistance | 1.87e+10 ohm @Time 86400 sec |
1.87e+10 ohm @Time 24.0 hour |
Control; IPC B24 |
Indium Corp. WF-9945 Wave Solder Flux, Halogen-Free WF-9945 is a halogen-free no-clean flux developed for wave soldering mixed-technology and through-hole electronics assemblies.WF-9945 is formulated to provide a excellent wetting and superior hole-f.. |