Electrical Properties Metric English Comments
Track Resistance >= 60000 sec
>= 60000 sec
inclined plane, 2500 volts
Bulk Molding Compounds BMC 5592 Arc, Track, and Weather Resistant Polyester
BMC 5592 molding compound is an arc, track and weather resistant grade polyester compound suitable for compression, transfer and stuffer injection molding. It has excellent impact strength, flame re..