Electrical Properties Metric English Comments
Track Resistance 3600 - 36000 sec
3600 - 36000 sec
Average value: 22300 sec Grade Count:17
Overview of materials for Silicone Rubber
This property data is a summary of similar materials in the MatWeb database for the category "Silicone Rubber". Each property range of values reported is minimum and maximum values of appropriate Ma..