Electrical Properties Metric English Comments
Track Resistance 3000 sec
3000 sec
Inclined-Plane Tracking; ASTM D2303
Mar-Bal MB1000-10 Thermoset Polyester Composite Molding Compound
A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information pro..
Track Resistance 3000 sec
3000 sec
Inclined-Plane Tracking; ASTM D2303
Mar-Bal MB1000-15 Thermoset Polyester Composite Molding Compound
A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information pro..
Track Resistance 3000 sec
3000 sec
Inclined-Plane Tracking; ASTM D2303
Mar-Bal MB1000-25 Thermoset Polyester Composite Molding Compound
A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information pro..