Electrical Properties | Metric | English | Comments |
---|---|---|---|
Track Resistance | 25200 sec | 25200 sec | 1 in @ 2.5 kV; ASTM D2303 |
3M BBI-A Shrinkable Tubing for Bus Bar 3M Heat Shrinkable Tubing for Bus Bar BBI-A Series is designed for insulating rectangular, square and round bus bar rated from 5 kV through 35 kV. It will also cover and insulate inline bolted conne.. |