Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Track Resistance 25 sec
25 sec
Bulk Molding Compounds BMC 1454 for Injection Molding Circuit Breakers
BMC 1454 is a special low-cost material developed specifically for injection molding circuit breakers. It has considerable flame, arc and track resistance. BMC 1454 is a medium strength material wit..