Electrical Properties Metric English Comments
Track Resistance 18000 sec
18000 sec
3.5 kV; ASTM 2303
3M 7620-S Cold Shrink QT-III Silicone Rubber Skirted Termination Kits
3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7620-S, 7680-S and 7690-S Series, contain one-piece, skirted, silicone Rubber Skirted Terminations, qualified as IEEE Standard 48 Cl..
Track Resistance 18000 sec
18000 sec
3.5 kV; ASTM 2303
3M 7620-T Cold Shrink Silicone Rubber Termination Kits QT-III
3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7620-Tand 7690-T Series, contain one-piece, non-skirted, silicone rubber termination, qualified as IEEE Standard 48 Class 1 for indo..
Track Resistance 18000 sec
18000 sec
3.5 kV; ASTM 2303
3M 7660-S Cold Shrink Silicone Rubber Termination Kits QT-III
3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7640-S, 7650-S and 7660-S Series, contains one-piece, skirted, silicone rubber termination, qualified as IEEE Standard 48 Class 1 fo..
Track Resistance 18000 sec
18000 sec
3.5 kV; ASTM 2303
3M 7680-S Cold Shrink QT-III Silicone Rubber Skirted Termination Kits
3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7620-S, 7680-S and 7690-S Series, contain one-piece, skirted, silicone Rubber Skirted Terminations, qualified as IEEE Standard 48 Cl..
Track Resistance 18000 sec
18000 sec
3.5 kV; ASTM 2303
3M 7690-T Cold Shrink Silicone Rubber Termination Kits QT-III
3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7620-Tand 7690-T Series, contain one-piece, non-skirted, silicone rubber termination, qualified as IEEE Standard 48 Class 1 for indo..
Track Resistance 18000 sec
18000 sec
3.5 kV; ASTM 2303
3M 7640-S Cold Shrink Silicone Rubber Termination Kits QT-III
3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7640-S, 7650-S and 7660-S Series, contains one-piece, skirted, silicone rubber termination, qualified as IEEE Standard 48 Class 1 fo..
Track Resistance 18000 sec
18000 sec
3.5 kV; ASTM 2303
3M 7650-S Cold Shrink Silicone Rubber Termination Kits QT-III
3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7640-S, 7650-S and 7660-S Series, contains one-piece, skirted, silicone rubber termination, qualified as IEEE Standard 48 Class 1 fo..
Track Resistance 18000 sec
18000 sec
3.5 kV; ASTM 2303
3M 7690-S Cold Shrink QT-III Silicone Rubber Skirted Termination Kits
3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7620-S, 7680-S and 7690-S Series, contain one-piece, skirted, silicone Rubber Skirted Terminations, qualified as IEEE Standard 48 Cl..