Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 1.00e+10 ohm @Temperature 23.0 °C |
1.00e+10 ohm @Temperature 73.4 °F |
50%RH; IEC 60167 |
DuPont Performance Polymers Zytel® 7301 NC010 Nylon 6
(Unverified Data**) Zytel® 7301 NC010 is a general purpose, unlubricated polyamide 6 resin for extrusion applications.Information provided by DuPont Performance Polymers |