Polymer Property : Electrical Resistivity = 8.00e+10 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 8.00e+10 ohm-cm

@Temperature 93.3 °C
8.00e+10 ohm-cm

@Temperature 200 °F
Abatron AboCast 8-4/Abocure 8-4 Epoxy  (discontinued **)
2-part solvent-free dielectric epoxy casting compound.Processing: 100/60 ratio (pbw); Gel time, 100 g (3.5 oz.): 240 minutes; cures in 3 weeks at 25°C (77°F).Applications: solventless casting, adh..