Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 5.00 ohm-cm @Temperature 1000 °C |
5.00 ohm-cm @Temperature 1830 °F |
|
MarkeTech Ceraflex 8Y Thin Zirconia Ceramic Oxygen Ion Conductor, Yttria Stabilized Data provided by the supplier, MarkeTech International.8 mole% Y2O3 (13.8 wt%). CERAFLEX is a sintered and fully dense zirconia ceramic material that is formed into extremely thin sheets, that are .. |