Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 2.00e+11 ohm-cm @Temperature 93.3 °C |
2.00e+11 ohm-cm @Temperature 200 °F |
|
Abatron AboCast 8-16/Abocure 8-16 Epoxy
(discontinued **) 2-part, clear, solvent-free dielectric epoxy casting compound.Processing: 100/35.00 ratio (pbw); Gel time, 100 g (3.5 oz.): 57 minutes; cures in 2 weeks at 25°C (77°F).Applications: solventless ca.. |