Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00013217 ohm-cm @Temperature 700 °C |
0.00013217 ohm-cm @Temperature 1290 °F |
|
Special Metals INCONEL® alloy N06230 Ni-Cr-W-Mo Alloy INCONEL® alloy N06230 (UNS N06230 / W.Nr. 2.4733) is a carbide strengthened nickel-chromium-tungsten-molybdenum alloy with an exceptional combination of strength, stability, and resistance to cor.. |