Electrical Properties Metric English Comments
Electrical Resistivity 0.00013085 ohm-cm

@Temperature 800 °C
0.00013085 ohm-cm

@Temperature 1470 °F
Special Metals INCONEL® alloy N06230 Ni-Cr-W-Mo Alloy
INCONEL® alloy N06230 (UNS N06230 / W.Nr. 2.4733) is a carbide strengthened nickel-chromium-tungsten-molybdenum alloy with an exceptional combination of strength, stability, and resistance to cor..