Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.000127 ohm-cm @Temperature 200 °C |
0.000127 ohm-cm @Temperature 392 °F |
|
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Bar, Hot Rolled and Solution Annealed HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Electrical Resistivity | 0.000127 ohm-cm @Temperature 200 °C |
0.000127 ohm-cm @Temperature 392 °F |
|
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Shielded Metal Arc Welded (SMAW) Plate HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Electrical Resistivity | 0.000127 ohm-cm @Temperature 500 °C |
0.000127 ohm-cm @Temperature 932 °F |
|
Haynes Hastelloy® C-22® alloy, 0% cold worked sheet HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Electrical Resistivity | 0.000127 ohm-cm @Temperature 500 °C |
0.000127 ohm-cm @Temperature 932 °F |
|
Haynes Hastelloy® C-22® alloy, 0.71-3.2 mm thick sheet, solution heat treated HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Electrical Resistivity | 0.000127 ohm-cm @Temperature 500 °C |
0.000127 ohm-cm @Temperature 932 °F |
|
Haynes Hastelloy® C-22® alloy, 20% cold worked sheet, aged 100 hours at 500°C HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Electrical Resistivity | 0.000127 ohm-cm @Temperature 500 °C |
0.000127 ohm-cm @Temperature 932 °F |
|
Haynes Hastelloy® C-22® alloy, 30% cold worked sheet HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Electrical Resistivity | 0.000127 ohm-cm @Temperature 500 °C |
0.000127 ohm-cm @Temperature 932 °F |
|
Haynes Hastelloy® C-22® alloy, 40% cold worked sheet, aged 100 hours at 500°C HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Electrical Resistivity | 0.000127 ohm-cm @Temperature 500 °C |
0.000127 ohm-cm @Temperature 932 °F |
|
Haynes Hastelloy® C-22® alloy, GTAW, aged 4000 hours at 450°C (800°F), notched HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Electrical Resistivity | 0.000127 ohm-cm @Temperature 500 °C |
0.000127 ohm-cm @Temperature 932 °F |
|
Haynes Hastelloy® C-22® alloy, GTAW, as welded, notched HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Electrical Resistivity | 0.000127 ohm-cm @Temperature 500 °C |
0.000127 ohm-cm @Temperature 932 °F |
|
Haynes Hastelloy® C-22® alloy, SMAW weld, 316L base metal, C-22 weld metal HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Electrical Resistivity | 0.000127 ohm-cm @Temperature 500 °C |
0.000127 ohm-cm @Temperature 932 °F |
|
Haynes Hastelloy® C-22® alloy, SMAW weld, C-22 base metal, C-22 weld metal HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Electrical Resistivity | 0.000127 ohm-cm @Temperature 500 °C |
0.000127 ohm-cm @Temperature 932 °F |
|
Haynes Hastelloy® C-22® alloy, transverse, GMAW spray weldment, 23.4 mm thick plate HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Electrical Resistivity | 0.000127 ohm-cm @Temperature 300 °C |
0.000127 ohm-cm @Temperature 572 °F |
|
Haynes Hastelloy® C-4 alloy, all-weld metal, as welded, GTAW Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) rang.. |
|||
Electrical Resistivity | 0.000127 ohm-cm @Temperature 300 °C |
0.000127 ohm-cm @Temperature 572 °F |
|
Haynes Hastelloy® C-4 alloy, welded plate 12.7 mm (1/2 in.) thick, aged 1000 hours at 649°C (1200°F) Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) rang.. |
|||
Electrical Resistivity | 0.000127 ohm-cm @Temperature 200 °C |
0.000127 ohm-cm @Temperature 392 °F |
|
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Sheet, Cold Rolled and Solution Annealed HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Electrical Resistivity | 0.000127 ohm-cm @Temperature 100 °C |
0.000127 ohm-cm @Temperature 212 °F |
|
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Electrical Resistivity | 0.000127 ohm-cm @Temperature 538 °C |
0.000127 ohm-cm @Temperature 1000 °F |
|
Carlson C 825 Nickel-Iron-Chromium Alloy General DescriptionCarlson Alloy C 825 is a nickel-iron-chromium alloy, developed for use in extremely corrosive environments. The nickel content of this alloy makes it resistant to chloride-ion st.. |
|||
Electrical Resistivity | 0.000127 ohm-cm @Temperature 500 °C |
0.000127 ohm-cm @Temperature 932 °F |
|
ATI Allegheny Ludlum Altemp® HX Nickel-Based superalloy Characteristics: outstanding resistance to oxidation at high temperatures, exceptional strength at elevated temperatures, good fabricability, good machinability in annealed condition, work hardening.. |
|||
Electrical Resistivity | 0.000127 ohm-cm @Temperature 500 °C |
0.000127 ohm-cm @Temperature 932 °F |
|
Haynes Hastelloy® C-22® alloy, all-weld metal, SMAW HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Electrical Resistivity | 0.000127 ohm-cm @Temperature 500 °C |
0.000127 ohm-cm @Temperature 932 °F |
|
Haynes Hastelloy® C-22® alloy, GTAW weld, 904L base metal, C-22 weld metal HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Electrical Resistivity | 0.000127 ohm-cm @Temperature 500 °C |
0.000127 ohm-cm @Temperature 932 °F |
|
Haynes Hastelloy® C-22® alloy, GTAW, as welded, unnotched HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Electrical Resistivity | 0.000127 ohm-cm @Temperature 500 °C |
0.000127 ohm-cm @Temperature 932 °F |
|
Haynes Hastelloy® C-22® alloy, transverse, GTAW short arc weldment, plate HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Electrical Resistivity | 0.000127 ohm-cm @Temperature 500 °C |
0.000127 ohm-cm @Temperature 932 °F |
|
Haynes Hastelloy® C-22® alloy, transverse, GTAW spray weldment, 12.7 mm (1/2 in.) thick plate HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Electrical Resistivity | 0.000127 ohm-cm @Temperature 300 °C |
0.000127 ohm-cm @Temperature 572 °F |
|
Haynes Hastelloy® C-4 alloy, sheet, aged 100 hours at 899°C Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) range. T.. |
|||
Electrical Resistivity | 0.000127 ohm-cm @Temperature 100 °C |
0.000127 ohm-cm @Temperature 212 °F |
|
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Plate, Hot Rolled and Solution Annealed HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing spe.. |
|||
Electrical Resistivity | 0.000127 ohm-cm @Temperature 100 °C |
0.000127 ohm-cm @Temperature 212 °F |
|
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing spe.. |
|||
Electrical Resistivity | 0.000127 ohm-cm @Temperature 500 °C |
0.000127 ohm-cm @Temperature 932 °F |
|
Haynes Hastelloy® C-22® alloy, 0% cold worked sheet, aged 100 hours at 500°C HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Electrical Resistivity | 0.000127 ohm-cm @Temperature 500 °C |
0.000127 ohm-cm @Temperature 932 °F |
|
Haynes Hastelloy® C-22® alloy, 6.4-19.1 mm thick plate, solution heat treated HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Electrical Resistivity | 0.000127 ohm-cm @Temperature 500 °C |
0.000127 ohm-cm @Temperature 932 °F |
|
Haynes Hastelloy® C-22® alloy, GTAW weld, 316L base metal, C-22 weld metal HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |