Polymer Property : Electrical Resistivity = 0.000121 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 0.000121 ohm-cm

@Temperature 300 °C
0.000121 ohm-cm

@Temperature 572 °F
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2025°F (1107°C)
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicat..
Electrical Resistivity 0.000121 ohm-cm

@Temperature 300 °C
0.000121 ohm-cm

@Temperature 572 °F
Haynes Hastelloy® G-35® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicat..
Electrical Resistivity 0.000121 ohm-cm

@Temperature 20.0 °C
0.000121 ohm-cm

@Temperature 68.0 °F
Haynes X-750 Nickel Alloy Sheet and Strip (AMS 5598, UNS N07750)
Haynes X-750 (UNS No. N07750) alloy is an age-hardenable, nickel-base superalloy with very good strength at temperatures up to about 1600°F (870°C). It is widely used as a wrought material for..
Electrical Resistivity 0.000121 ohm-cm

@Temperature 300 °C
0.000121 ohm-cm

@Temperature 572 °F
Haynes Hastelloy® G-35® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicat..
Electrical Resistivity 0.000121 ohm-cm

@Temperature 300 °C
0.000121 ohm-cm

@Temperature 572 °F
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2075°F (1135°C)
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicat..
Electrical Resistivity 0.000121 ohm-cm

@Temperature 300 °C
0.000121 ohm-cm

@Temperature 572 °F
Haynes Hastelloy® G-35® Nickel Alloy Sheet, Annealed at 2075°F (1135°C)
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is..
Electrical Resistivity 0.000121 ohm-cm

@Temperature 300 °C
0.000121 ohm-cm

@Temperature 572 °F
Haynes Hastelloy® G-35® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is..
Electrical Resistivity 0.000121 ohm-cm

@Temperature 300 °C
0.000121 ohm-cm

@Temperature 572 °F
Haynes Hastelloy® G-35® Nickel Alloy Bar, Annealed at 2075°F (1135°C)
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is..