Polymer Property : Electrical Resistivity = 0.000113 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 0.000113 ohm-cm

@Temperature 427 °C
0.000113 ohm-cm

@Temperature 801 °F
H.C. Starck MP35N® Nickel/Cobalt/Chromium/Molybdenum Alloy
MP35N is a nickel-cobalt based alloy of the Multiphase® alloy system that has ultra high strength, toughness, ductility, biocompatibility, and outstanding corrosion resistance. H.C. Starck offers..
Electrical Resistivity 0.000113 ohm-cm

@Temperature 25.6 °C
0.000113 ohm-cm

@Temperature 78.0 °F
Carlson C 825 Nickel-Iron-Chromium Alloy
General DescriptionCarlson Alloy C 825 is a nickel-iron-chromium alloy, developed for use in extremely corrosive environments. The nickel content of this alloy makes it resistant to chloride-ion st..
Electrical Resistivity 0.000113 ohm-cm

@Temperature 400 °C
0.000113 ohm-cm

@Temperature 752 °F
Temperature resistance factor (F) =1.045
Alloy Wire International RW 80 Ni-Cr Resistance Wire
Used in heating elements and control resistors because of its electrical properties and resistance to oxidation under temperature cycling and frequent switching. Also used in hot cutting operations..