Polymer Property : Electrical Resistivity = 0.000112 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 0.000112 ohm-cm

@Temperature 200 °C
0.000112 ohm-cm

@Temperature 392 °F
Haynes 75 Nickel Alloy Sheet, Annealed at 1925°F (1050°C)
Haynes alloy 75 is a solution-strengthened nickel-chromium alloy with moderate strength to 1200°F (650°C). It is principally used in low stress elevated temperature applications requiring reas..
Electrical Resistivity 0.000112 ohm-cm

@Temperature 400 °C
0.000112 ohm-cm

@Temperature 752 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) All Weld Cruciform
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Electrical Resistivity 0.000112 ohm-cm

@Temperature 400 °C
0.000112 ohm-cm

@Temperature 752 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Electrical Resistivity 0.000112 ohm-cm

@Temperature 400 °C
0.000112 ohm-cm

@Temperature 752 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) Sheet
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Electrical Resistivity 0.000112 ohm-cm

@Temperature 400 °C
0.000112 ohm-cm

@Temperature 752 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate and Bar, Hot-rolled, Solution Annealed
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Electrical Resistivity 0.000112 ohm-cm

@Temperature 400 °C
0.000112 ohm-cm

@Temperature 752 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate, Age-hardened
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Electrical Resistivity 0.000112 ohm-cm

@Temperature 400 °C
0.000112 ohm-cm

@Temperature 752 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate, Annealed
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Electrical Resistivity 0.000112 ohm-cm

@Temperature 400 °C
0.000112 ohm-cm

@Temperature 752 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Sheet, Cold-rolled, Solution Annealed
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Electrical Resistivity 0.000112 ohm-cm

@Temperature 400 °C
0.000112 ohm-cm

@Temperature 752 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Sheet, Cold-rolled, Solution Annealed, Age-hardened
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Electrical Resistivity 0.000112 ohm-cm

@Temperature 400 °C
0.000112 ohm-cm

@Temperature 752 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Electrical Resistivity 0.000112 ohm-cm

@Temperature 400 °C
0.000112 ohm-cm

@Temperature 752 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate and Bar, Hot-rolled, Solution Annealed, Age-hardened
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately doubl..
Electrical Resistivity 0.000112 ohm-cm

@Temperature 400 °C
0.000112 ohm-cm

@Temperature 752 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately doubl..
Electrical Resistivity 0.000112 ohm-cm

@Temperature 204 °C
0.000112 ohm-cm

@Temperature 399 °F
ATI Allegheny Ludlum ALFA-I™ Stainless Steel Type 406
Characteristics:superior oxidation resistance for the temperature range 1600°F-over 2200°F, high electrical resistivity, high resistance to sulfidation, high resistance to carburization. Applicat..