Polymer Property : Electrical Resistivity = 0.000111 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 0.000111 ohm-cm

@Temperature 300 °C
0.000111 ohm-cm

@Temperature 572 °F
Temperature resistance factor (F) =1.028
Alloy Wire International RW 80 Ni-Cr Resistance Wire
Used in heating elements and control resistors because of its electrical properties and resistance to oxidation under temperature cycling and frequent switching. Also used in hot cutting operations..
Electrical Resistivity 0.000111 ohm-cm

@Temperature 700 °C
0.000111 ohm-cm

@Temperature 1290 °F
ATI Allegheny Ludlum AL 403™ Martensitic Stainless Steel
Characteristics: corrosion resistant, heat resistant, oxidation resistant up to 1400°F.Information provided by Allegheny Ludlum
Electrical Resistivity 0.000111 ohm-cm

@Temperature 20.0 °C
0.000111 ohm-cm

@Temperature 68.0 °F
ATI Allegheny Ludlum ALFA-I™ Stainless Steel Type 406
Characteristics:superior oxidation resistance for the temperature range 1600°F-over 2200°F, high electrical resistivity, high resistance to sulfidation, high resistance to carburization. Applicat..