Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.000109 ohm-cm @Temperature 100 °C |
0.000109 ohm-cm @Temperature 212 °F |
Temperature resistance factor (F) =1.006 |
Alloy Wire International RW 80 Ni-Cr Resistance Wire Used in heating elements and control resistors because of its electrical properties and resistance to oxidation under temperature cycling and frequent switching. Also used in hot cutting operations.. |