Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0001035 ohm-cm @Temperature 600 °C |
0.0001035 ohm-cm @Temperature 1110 °F |
|
ATI Allegheny Ludlum AL 403™ Martensitic Stainless Steel Characteristics: corrosion resistant, heat resistant, oxidation resistant up to 1400°F.Information provided by Allegheny Ludlum |