Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0000880 ohm-cm @Temperature 400 °C |
0.0000880 ohm-cm @Temperature 752 °F |
|
ATI Allegheny Ludlum AL 403™ Martensitic Stainless Steel Characteristics: corrosion resistant, heat resistant, oxidation resistant up to 1400°F.Information provided by Allegheny Ludlum |