Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0000720 ohm-cm @Temperature 23.0 °C |
0.0000720 ohm-cm @Temperature 73.4 °F |
|
Crucible Steel 431 Chromium Steel Crucible 431 is a nickel bearing chromium steel which can be treated to exceptionally high physical properties. In the heat treated conditions, its corrosion resistance is superior to similar marten.. |
|||
Electrical Resistivity | 0.0000720 ohm-cm @Temperature 23.0 °C |
0.0000720 ohm-cm @Temperature 73.4 °F |
|
Crucible Steel 431 Chromium Steel Crucible 431 is a nickel bearing chromium steel which can be treated to exceptionally high physical properties. In the heat treated conditions, its corrosion resistance is superior to similar marten.. |
|||
Electrical Resistivity | 0.0000720 ohm-cm @Temperature 200 °C |
0.0000720 ohm-cm @Temperature 392 °F |
|
ATI Allegheny Ludlum AL 403™ Martensitic Stainless Steel Characteristics: corrosion resistant, heat resistant, oxidation resistant up to 1400°F.Information provided by Allegheny Ludlum |