Polymer Property : Electrical Resistivity = 0.0000500 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000500 ohm-cm

@Temperature 20.0 °C
0.0000500 ohm-cm

@Temperature 68.0 °F
Bohler-Uddeholm BÖHLER W303 ISODISC® Hot Work Tool Steel
Description: Hot work tool steel featuring excellent hot tensile properties, high retention of hardness, good toughness and resistance to heat checking, admits water cooling. BOHLER W303 is also ava..
Electrical Resistivity 0.0000500 ohm-cm

@Temperature 20.0 °C
0.0000500 ohm-cm

@Temperature 68.0 °F
Bohler-Uddeholm BÖHLER W403 VMR® Hot Work Tool Steel
W403 VMR is a modified hot work alloy with an excellent combination of hot tensile properties and toughness. The balanced properties of this grade are not only due to chemistry modification, but to ..