Polymer Property : Surface Resistance = 9.90e+12 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistance 10.0 - 9.90e+12 ohm
10.0 - 9.90e+12 ohm
Average value: 5.55e+11 ohm Grade Count:10
Overview of materials for Styrenic Elastomer (TES)
This property data is a summary of similar materials in the MatWeb database for the category "Styrenic Elastomer (TES)". Each property range of values reported is minimum and maximum values of appro..