Polymer Property : Surface Resistance = 9.00e+12 ohm
Polymer Property :
Surface Resistance =
9.00e+12 ohm
Product List
Electrical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties
Metric
English
Comments
Surface Resistance
9.00e+12
ohm
9.00e+12
ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-LOY SLWM2105 PBT+PC (Asia Pacific)
Anti-static PBT/PC blend, mineral 5% filled product